Sains Malaysiana 43(1)(2014): 145–150

 

Direction of Flexoelectric Polarization in Smectic C*G Phases of

Chiral Smectic Liquid Crystals

(Arah Pengutuban Fleksoelektrik dalam Fasa Smektik C*G bagi Hablur Cecair Khiral Smektik)

 

TENG YONG TAN & LYE HOCK ONG*

School of Physics, Universiti Sains Malaysia, 11800 Minden, Penang, Malaysia

 

Received: 10 December 2012/Accepted: 14 March 2013

 

ABSTRACT

Polarization in antiferroelectric liquid crystals has two origins: The piezoelectric polarization which is of chiral origin and the flexoelectric polarization which originates in different orientation of tilts in neighboring layers. The flexoelectric polarization is perpendicular to the tilt direction only if the structure is uniformly helicoidally modulated. In structures like SmC*F11 and SmC*F12 the flexoelectric contribution might be significant and it can be non-parallel to the piezoelectric component. Hence it may deviates the direction of polarization from the perpendicular direction significantly. The angle formed by the polarization and the tilt is therefore general and as such the basic characteristic of the SmC*G phase can be recognized. It seems that this aspect was completely overlooked in the past. In this contribution we analyze the dependence of the polarization direction on the phase structures and on the values of piezoelectric and flexoelectric coefficients in the discrete phenomenological model.

 

Keywords: Antiferroelectric liquid crystals; general tilt phase; multilayer structure

 

ABSTRAK

Pengkutuban di dalam hablur cecair antiferoelektrik berasal daripada dua sumber berikut: pengkutuban piezoelektrik yang berasal daripada sifat khiralnya dan pengkutuban fleksoelektrik yang berasal daripada 'tilt-tilt' di dalam lapisan terdekat yang berada dalam orientasi yang berbeza. Pengkutuban fleksoelektrik adalah berserenjang kepada arah 'tilt' sahaja jika struktur yang dikaji berbentuk 'kelopak bunga' yang seragam. Dalam struktur seperti Sm*F11 dan SmC*F12, penyumbangan fleksoelektrik mungkin ketara dan ia adalah tidak selari kepada komponen piezoelektrik. Maka, ia mungkin menyimpangkan arah pengkutuban daripada arah berserenjang secara ketaranya. Sudut yang dibentuk daripada pengkutuban dan 'tilt' ini adalah dikatakan secara am dan ciri asal fasa SmC*G boleh dikenal pasti. Aspek ini tidak diambil kira sebelum ini. Dalam kertas ini, kami menganalisis arah pengkutuban dalam struktur tersebut berdasarkan pergantungan nilai parameter piezoelektrik dan fleksoelektrik dengan menggunakan model fenomenologi diskrit.

 

Kata kunci: Fasa 'tilt' am; hablur cecair antiferoelektrik; struktur berbilang lapis

REFERENCES

Bailey, C. & Jákli, A. 2007. Role of molecular shape on bent-core liquid-crystal structures. Physical Review Letters 99: 207801.

Brand, H.R., Cladis, P.E. & Pleiner, H. 1998. Macroscopic properties of smectic CG liquid crystals. European Physical Journal B 6: 347-353.

Čepič, M. & Žekš, B. 2001. Flexoelectricity and piezoelectricity: The reason for the rich variety of phases in antiferroelectric smectic liquid crystals. Physical Review Letters 87(8): 085501.

Chandani, A.D.L., Gorecka, E., Ouchi, Y., Takezoe, H. & Fukuda, A. 1989. Antiferroelectric chiral smectic phases responsible for the tristable switching in MHPOBC. Japanese Journal of Applied Physics 28(7): L1265-L1268.

Cladis, P.E., Brand, H.R. & Pleiner, H. 1999. Fluid biaxial banana smectics: Symmetry at work. Liquid Crystals Today 9(3-4): 1-6.

de Gennes, P.G. 1993. The Physics of Liquid Crystals. 2nd ed. Oxford: Clarendon Press.

Dolganov, P.V., Zhilin, V.M., Dmitrienko, V.E. & Kats, E.I. 2002. Polar smectic subphases: Phase diagrams, structures and x-ray scattering. Journal of Experimental and Theoretical Physics Letters 76(8): 498-501.

Fernandes, P., Barois, P., Grelet, E., Nallet, F., Goodby, J.W., Hird, M. & Micha, J-S. 2006. Extension of the resonant scattering technique to liquid crystals without resonant element. European Physical Journal E 20: 81-87.

Fukuda, A., Takanishi, Y., Isozaki, T., Ishikawa, K. & Takezoe, H. 1994. Antiferroelectric chiral smectic liquid crystals. Journal of Materials Chemistry 4(7): 997-1016.

Gorecka, E., Pociecha, D., Cepic, M., Žekš, B. & Dabrowski, R. 2002. Enantiomeric excess dependence of the phase diagram of antiferroelectric liquid crystals. Physical Review E 65: 061703.

Gorecka, E., Pociecha, D., Vaupotic, N., Cepic, M., Gomola, K. & Mieczkowski, J. 2008. Modulated general tilt structures in bent-core liquid crystals. Journal of Materials Chemistry 18: 3044-3049.

Lagerwall, S.T. 1999. Ferroelectric and Antiferroelectric Liquid Crystals. Weinheim: Wiley-VCH.

Muševic, I., Blinc, R. & Žekš, B. 2000. The Physics of Ferroelectric and Antiferroelectric Liquid Crystals. Singapore: World Scientific.

Niori, T., Sekine, T., Watanabe, J., Furukawa, T. & Takezoe, H. 1996. Distinct ferroelectric smectic liquid crystals consisting of banana shaped achiral molecules. Journal of Materials Chemistry 6(7): 1231-1233.

Pikin, S.A. & Indebom, V.L. 1978. Thermodynamic states and symmetry of liquid crystals. Soviet Physics Uspekhi 21(6): 487-501.

Takezoe, H., Gorecka, E. & Cepic, M. 2010. Antiferroelectric liquid crystals: Interplay of simplicity and complexity. Reviews of Modern Physics 82(1): 897-937.

 

*Pengarang untuk surat-menyurat; e-mail: onglh@usm.my