Sains Malaysiana 49(12)(2020): 3045-3054
http://dx.doi.org/10.17576/jsm-2020-4912-16
Effect of Isothermal Aging
and Copper Substrate Roughness on the SAC305 Solder Joint Intermetallic Layer Growth
of High Temperature Storage (HTS)
(Kesan Penuaan Isoterma dan
Kekasaran Permukaan Substrat Kuprum ke atas Pertumbuhan Lapisan antara Logam Sambungan Pateri SAC305 pada
Penyimpanan Suhu Tinggi (HTS))
RABIAH AL ADAWIYAH AB RAHIM1,
MUHAMMAD NUBLI ZULKIFLI2, AZMAN JALAR1,3*,
ATIQAH MOHD AFDZALUDDIN1 & KIM SIOW SHYONG1
1Institute of
Microengineering and Nanoelectronics (IMEN), Universiti Kebangsaan Malaysia, 43600
UKM Bangi, Selangor Darul Ehsan, Malaysia
2Universiti Kuala
Lumpur (UniKL), British Malaysia Institute (BMI), Electrical Engineering
Section, Jalan Sungai Pusu, 53100 Gombak, Selangor Darul Ehsan, Malaysia
3Department of Applied Physics, Faculty of Science & Technology,
Universiti Kebangsaan Malaysia, 43600 UKM Bangi, Selangor Darul Ehsan, Malaysia
Received: 13 August 2020/Accepted:
27 August 2020
ABSTRACT
This study aims to evaluate the effect of
copper (Cu) substrate surface roughness on the intermetallic compound (IMC)
growth and interfacial reaction of SAC305 lead-free solder joint after
undergone an aging process. Aging process was conducted using high temperature
storage (HTS) at temperature of 150 °C and aging times of 200, 400, 600, 800,
and 1000 h. IMC morphology and growth were examined using infinite focus
microscope (IFM). Then, the SAC305 solder joint IMC growth kinetic was measured
based on power law relationship and diffusion coefficient formula. It was noted
that the morphology of IMC for the rougher Cu substrate has scallop-shaped and
uniform layer as compared to that of smoother Cu substrate for the initial
exposure to the HTS. In addition, Cu
substrate with Ra of 579 nm is the turning point for the creation of
Cu6Sn5 towards more Cu3Sn of IMC. In addition,
Cu substrate with Ra of 579 nm also acts as the turning point for
the IMC growth of SAC305 solder joint on Cu substrate for the solid-state
diffusion to be happened during 150 °C of aging from grain boundary dominant
toward volume diffusion dominant.
Keywords: High temperature storage (HTS); IMC
layer growth, IMC thickness; SAC305 solder; substrate roughness
ABSTRAK
Kajian ini
bertujuan untuk menilai kesan kekasaran permukaan substrat kuprum (Cu) ke atas
pertumbuhan lapisan sebatian antara logam (IMC) dan tindak balas antara muka
sambungan pateri SAC305 selepas melalui proses penuaan. Proses penuaan
dijalankan menggunakan penyimpanan suhu tinggi (HTS) pada suhu 150 °C dan masa
penuaan 200, 400, 600, 800 dan 1000 jam. Morfologi dan pertumbuhan IMC dicerap
menggunakan mikroskop fokus tak terjangka (IFM). Kemudian, pertumbuhan kinetik
sambungan pateri SAC305 diukur berdasarkan hubungan hukum kuasa dan formula
pekali resapan. Morfologi IMC untuk substrat Cu yang lebih kasar menunjukkan ia
berbentuk kerangan dan lapisan yang seragam berbanding substrat Cu yang lebih
licin untuk permulaan pendedahan kepada HTS. Sebagai tambahan, substrat Cu
dengan 579 nm Ra merupakan titik permulaan kepada pertumbuhan IMC
sambungan pateri SAC305 di atas substrat Cu untuk resapan keadaan pepejal berlaku
semasa penuaan 150 °C daripada dominan sempadan terhadap dominan resapan isi
padu.
Kata kunci: Kekasaran substrat; ketebalan IMC;
penyimpanan suhu tinggi (HTS); pertumbuhan lapisan IMC; pateri SAC305
REFERENCES
Abu
Bakar, M., Azman, J., Roslina, I. & Abdul, R.D. 2016. Nanoindentation of
Sn3Ag0. 5Cu/ENIG solder joint after high temperature storage. Materials
Science Forum 857: 40-43.
Anon. N.D.R. 2020. RMS Surface Roughness
Calculation - Surface Finish Formulas, Harrison Electropolishing. http://www.harrisonep.com/electropolishing-ra.html. Accessed on 26 August 2020.
Bhat, K.N., Prabhu, K.N. & Satyanarayan. 2014. Effect of reflow
temperature and substrate roughness on wettability, IMC growth and shear
strength of SAC387/Cu bonds. Journal of Materials Science: Materials in
Electronics 25(2): 864-872.
Hu, X., Xu, T., Keer, L.M., Li, Y. & Jiang, X. 2016.
Microstructure evolution and shear fracture behavior of aged Sn3Ag0.5Cu/Cu
solder joints. Materials Science and Engineering: A 673: 167-177.
Ismail, N., Jalar, A., Abu Bakar, M. & Ismail, R. 2018a. Kesan
penambahan tiubnano karbon terhadap pertumbuhan lapisan sebatian antara logam
sistem pateri Sn-Ag-Cu/Cu akibat penuaan terma. Sains Malaysiana 47(7):
1585-1590.
Ismail, N., Ismail, R., Jalar, A., Omar, G., Salleh, E.M., Kamil, N.
& Rahman, I.A. 2018b. Comparative study of interfacial interaction between
aromatic and aliphatic functional group in solder wettability. Journal of
Materials Science: Materials in Electronics 29(15): 12910-12916.
Ismail, N., Ismail, R., Nik Ubaidillah, N.K.A., Jalar, A. & Zain,
N.M. 2016a. Surface roughness and wettability of SAC/CNT lead free solder. Materials
Science Forum 857: 73-75.
Ismail, N., Ismail, R., Abd Aziz, N.I. & Jalar, A. 2016b.
Wettability of CNT-doped solder under isothermal aging. Materials Science
Forum 857: 76-78.
Jalar, A., Abu Bakar, M., Ismail, R. & Abdul, R.D. 2016.
Statistical aspect on the measuring of intermetallic compound thickness of lead
free solders. Journal of Scientific Research and Development 3(4):
49-54.
Jiang, N., Zhang, L., Liu, Z-Q., Sun, L., Long, W-M., He, P., Xiong,
M-Y. & Zhao, M. 2019. Reliability issues of lead-free solder joints in
electronic devices. Science and Technology of Advanced Materials 20(1):
876-901.
Lee, J-H. & Kim, Y-J. 2014. Hydroxyapatite nano fibers fabricated
through electrospinning and sol-gel process. Ceramics International 40(2): 3361-3369.
Lee, L.M. & Ahmad, A.M. 2013. Interfacial reaction of Sn-Ag-Cu
lead-free solder alloy on Cu: A review. Advances in Materials Science and
Engineering 2013: Article ID. 123697.
Li, H., An, R., Wang, C. & Jiang, Z. 2015. In situ quantitative study of microstructural evolution at the
interface of Sn3.0Ag0.5Cu/Cu solder joint during solid state aging. Journal
of Alloys and Compounds 634: 94-98.
Liu, J., Zhao, H., Li, Z., Song, X., Zhao, Y., Niu, H., Tian, H.,
Dong, H. & Feng, J. 2018. Microstructure evolution, grain morphology
variation and mechanical property change of Cu-Sn intermetallic joints
subjected to high-temperature aging. Materials Characterization 135(November): 238-244.
Mo, L., Wu, F. & Liu, C. 2015. Growth kinetics of IMCs in Cu-Sn
intermetallic joints during isothermal soldering process. Proceedings -
Electronic Components and Technology Conference. pp. 1854-1858.
Rabiatul Adawiyah, M.A. & Saliza Azlina, O. 2018. Comparative
study on the isothermal aging of bare Cu and ENImAg surface finish for Sn-Ag-Cu
solder joints. Journal of Alloys and Compounds 740: 958-966.
Satyanarayan & Prabhu, K.N. 2013. Spreading behavior and evolution
of IMCs during reactive wetting of sac solders on smooth and rough copper
substrates. Journal of Electronic Materials 42(8): 2696-2707.
Tang, Y., Luo, S.M., Li, Z.H., Hou, C.J. & Li, G.Y. 2018.
Morphological evolution and growth kinetics of interfacial Cu 6 Sn 5 and Cu 3
Sn layers in low-Ag Sn-0.3 Ag-0.7 Cu-XMn/Cu solder joints during isothermal
ageing. Journal of Electronic Materials 47(10): 5913-5929.
Wang, C., Li, M., Chiu, C. & Chang, T. 2018. Kinetic study of
solid-state interfacial reactions of p-type (Bi, Sb) 2Te3 thermoelectric
materials with Sn and Sn–Ag–Cu solders. Journal of Alloys and Compounds 767: 1133-1140.
Wang, Y., Wang, G., Song, K. & Zhang, K. 2017. Effect of Ni
addition on the wettability and microstructure of Sn2.5Ag0.7Cu0.1RE solder
alloy. Materials & Design 119: 219-224.
Wu, Y., Jennifer, A.S., Cyrus, P., Ann Foster, L., Marshall, J.L.,
Jacobs, E.G. & Pinizzotto, R.F. 1993. The formation and growth of
intermetallics in composite solder. Journal of Electronic Materials 22(7):
769-777.
Xiao, H., Li, X.Y., Zhu, Y.X., Yang, J.L., Chen, J. & Guo, F.
2013. Intermetallic growth study on SnAgCu/Cu solder joint interface during
thermal aging. Journal of Materials Science: Materials in Electronics 24(7): 2527-2536.
Yang, M., Ko, Y-H., Bang, J., Kim, T-S., Lee, C-W. & Li, M. 2017.
Effects of Ag addition on solid–state interfacial reactions between Sn–Ag–Cu
solder and Cu substrate. Materials Characterization 124: 250-259.
Yu, D.Q., Wu, C.M.L., Law, C.M.T., Wang, L. & Lai, J.K.L. 2005. Intermetallic
compounds growth between Sn-3.5Ag lead-free solder and Cu substrate by dipping
method. Journal of Alloys and Compounds 392(1-2): 192-199.
Zhu, Z., Ma, H., Shang, S., Ma, H., Wang, Y. & Li, X. 2019. Effect
of polycrystalline Cu microstructures on IMC growth behavior at Sn/Cu soldering
interface. Journal of Materials Science: Materials in Electronics 30(17): 15964-15971.
*Corresponding author; email: azmn@ukm.edu.my
|